Specialist authority in maintaining and improving plastic injection machines Saturday to Wednesday, 8:00–17:00
Materials

Did you know that a part molded from undried material can look perfect while having lost much of its strength?

0.02%commonly recommended maximum moisture for polycarbonate before molding

In materials such as PC, PET and PBT, moisture breaks the polymer chains at melt temperature. The part has the right shape but cracks during assembly or under load.

This is hydrolysis: at high temperature water reacts with the polymer and lowers its molecular weight. Sometimes you see silver streaks or bubbles, but sometimes there is no visible sign and the problem only appears in an impact test or as a failure in the customer's hands.

The allowed moisture differs for each material and must be taken from the supplier's datasheet: for polycarbonate typically around 0.02%, and for PET even lower. An ordinary hot-air dryer can't reach this level; a desiccant dryer is required.

Over-drying isn't harmless either: some materials, such as polyamide, turn yellow with long, hot drying. Temperature and time should follow the datasheet, not "the more the better".

This article is general guidance. The figures depend on each plant's conditions; for decisions, measurements on your own line are what count.